That is very interesting and
surprising. High temperature visco-elastic creep. What is the
TOT? I wouldn’t have thought it high enough; but in any case, it
suggests that intergranular stress corrosion of the SS could also be
ocurring. It may be good to inspect the hottest portions of that pipe
fairly frequently.
Al