I think we all know by now the SS (including 321) is subject to stress
corrosion at the temperatures it sees in rotary near the engine.  First
choice - use inconel.  Second choice - make sure the SS is not subjected
to stress; i.e; use slips joints, flex bellows, whatever.

My $0.02 worth.