HDT is generally above the cure temp until the cure temp is the same temp.
----- Original Message -----
From: <Newlan2dl@aol.com>
To: "Lancair Mailing List" <lml@lancaironline.net>
Sent: Tuesday, August 27, 2002 8:54 AM
Subject: [LML] Re: Lancair Paint Colors
Hi Dan
Yes, I agree about the limitations on the skin temperatures of the prepregs
but those are probably around 260. I tried to get the exact HDT of Lancairs
prepreg but they didn't have it handy so I'll continue to research but it is
probably close to the cure temp. of 260 which is where I'd like the other
laminating resins to be. And I'd prefer they be toughened for better flex,
(and impact though that is probably never an issue) and reduced tendancy
for
fatigue.
Dan Newland
#############################################################
For archives see the LML website: http://www.lancaironline.net/maillist.html